Standard: EN 10130 · ASTM A1008/A1008M · JIS G3141 · IS 513 (Part 1) formerly DIN 1623-1, ASTM A366 / A619 / A620
Cold rolled low-carbon steels for forming are graded by how much forming they can take, from commercial quality to extra-deep drawing. The table lines up the grade names of the main standards; the steels are close but not identical, because the standards set different limits and test pieces — specify one standard on an order rather than “DC01 or equivalent”.
| Forming quality | EN 10130 | ASTM A1008 | JIS G3141 | IS 513 | Former DIN 1623 |
|---|---|---|---|---|---|
| Commercial | DC01 | CS Type B | SPCC | CR1 | St 12 |
| Drawing | DC03 | DS Type B | SPCD | CR2 | RRSt 13 |
| Deep drawing | DC04 | DDS | SPCE | CR3 | St 14 |
| Extra deep drawing | DC05 | EDDS | SPCF | CR4 | – |
| Extra deep drawing, interstitial-free | DC06 | EDDS | SPCG | CR5 | – |
| Purpose | EN | ASTM | JIS |
|---|---|---|---|
| Vitreous enamelling | EN 10209 DC01EK, DC04EK, DC06EK | A424 Type I–III | G3133 SPP |
| High-strength low-alloy for cold forming | EN 10268 HC260LA–HC420LA | A1008 HSLAS | G3135 SPFC |
| Structural | EN 10025-2 S235–S355 (hot rolled grades) | A1008 SS Grade 25–80 | – |
Translation isn’t available right now. The site is shown in English.